Physico-chemical characterization of functional electrospun scaffolds for bone and cartilage tissue engineering
Authors:
- 29 July 2010
- journal article
- other
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 224 (12) , 1401-1414
Abstract
Mimicking the zonal organization of the bone–cartilage interface will aid the production of functional osteochondral grafts for regeneration of skeletal joint defects. This study investigates the potential of the electrospinning technique to build a three-dimensional construct recapitulating the zonal matrix of this interface. Poly(lactic- co-glycolic acid) (PLGA) and PLGA–collagen solutions containing different concentrations of hydroxyapatite nanoparticles (nHAp) were electrospun on a thin layer of phosphate buffer saline solution spread on the collector in order to facilitate membrane detachment and recovery. Incorporation of increasing amounts of nHAp in PLGA solutions did not affect significantly the average diameter of the fibres, which was about 700 nm. However, in the presence of collagen, fibres with diameters below 100 nm were generally observed and the number of these fibres was inversely proportional to the ratio PLGA:collagen and proportional to the content of nHAp. PLGA membranes were rather hydrophobic, although the aqueous drop contact angles progressively fell from 125° to 110° when the content of nHAp was increased from 0 per cent to 50 per cent (w/v). PLGA–collagen membranes were more hydrophilic with contact angles between 60° and 110°; the values being proportional to the ratio PLGA:collagen and the content of nHAp. Also, the addition of nHAp from 0 per cent to 50 per cent (w/v) in the absence of collagen resulted in decreasing dramatically both the Young's modulus ( Ym), from 34.3 ± 1.8 MPa to 0.10 ± 0.06 MPa, and the ultimate tensile strain ( εmax), from a value higher than 40 per cent to 5 per cent. However, the presence of collagen together with nHAp allowed the creation of membranes much stiffer, although more brittle, as shown for membranes made with a ratio 8:2 and 10 per cent of nHAp, for which Ym = 70.0 ± 6.6 MPa and εmax = 7 per cent.Keywords
This publication has 23 references indexed in Scilit:
- Influence of Scaffold Stiffness on Subchondral Bone and Subsequent Cartilage Regeneration in an Ovine Model of Osteochondral Defect HealingThe American Journal of Sports Medicine, 2008
- Engineering custom-designed osteochondral tissue graftsTrends in Biotechnology, 2008
- Repair of porcine articular cartilage defect with a biphasic osteochondral compositeJournal of Orthopaedic Research, 2007
- Osteochondral repair in the rabbit model utilizing bilayered, degradable oligo(poly(ethylene glycol) fumarate) hydrogel scaffoldsJournal of Biomedical Materials Research Part A, 2005
- Current strategies for articular cartilage repair2005
- Tissue engineering of biphasic cartilage constructs using various biodegradable scaffolds: an in vitro studyBiomaterials, 2004
- In vitro generation of osteochondral compositesBiomaterials, 2000
- Review: tissue engineering for regeneration of articular cartilageBiomaterials, 2000
- A novel osteochondral implantBiomaterials, 1999
- Subchondral bone and cartilage repair with bioactive glasses, hydroxyapatite, and hydroxyapatite-glass compositeJournal of Biomedical Materials Research, 1996