Molecular Mobility and Phase Structure of Biodegradable Poly(butylene succinate) and Poly(butylene succinate-co-butylene adipate)

Authors:

Abstract
Molecular mobility and phase structure of biodegradable poly(butylene succinate) (PBS) and poly(butylene succinate-co-20 mol % butylene adipate) [P(BS-co-20 mol % BA)] have been investigated by high-resolution solid-state 13C NMR. For both samples, two components with different 13C spin−lattice relaxation time (T1C) values have been observed in the crystalline region. The crystalline component with shorter T1C value is assignable to the interface near amorphous phase. The crystalline component with longer T1C value is ascribed to the inside of the crystalline region. On the basis of T1C, it has been concluded that the BA units are not included in the crystalline region of P(BS-co-20 mol % BA). Molecular mobility and higher-ordered structure of amorphous phase have been also compared between the melt and solid state. Variable-temperature high-resolution 13C NMR measurements for the amorphous phase have revealed the remarkable difference in dynamics and structure between the melt and solid state.

This publication has 39 references indexed in Scilit: