Sintering of cubic boron nitride without additives at 7.7 GPa and above 2000 °C
Authors:
- 1 January 1999
- journal article
- Published by Springer Nature in Journal of Materials Research
- Vol. 14 (1) , 162-169
Abstract
The sintering behavior of cBN powder with various particle sizes from 0.5 to 12 µm was investigated when sintered at temperatures from 1500 to 2500 °C and pressure of 7.7 GPa without additives. Above 2000 °C, translucent sintered bodies were obtained. Microstructure observation indicated that the optimum sintering temperature was near 2350 °C for fine powders of 0.5 to 1.2 µm and 2 to 4 µm, and slightly higher than 2350 °C for powders from 8 to 12 µm. The fracture toughness of the well-sintered bodies decreased with grain growth above the optimum sintering temperature.Keywords
This publication has 7 references indexed in Scilit:
- Mechanical Properties of Polycrystalline Translucent Cubic Boron Nitride as Characterized by the Vickers Indentation MethodJournal of the American Ceramic Society, 1996
- Mechanical properties of diamond and cubic BN at different temperatures and deformation ratesDiamond and Related Materials, 1993
- Synthesis of translucent sintered cubic boron nitrideJournal of Materials Science Letters, 1993
- Sintered Superhard MaterialsScience, 1980
- Fracture Toughness Determinations by IndentationJournal of the American Ceramic Society, 1976
- Direct transitions among the allotropic forms of boron nitride at high pressures and temperaturesThe Journal of Chemical Physics, 1975
- Synthesis of polycrystalline cubic BNMaterials Research Bulletin, 1972