Impact of Precursor Chemistry and Process Conditions on the Scalability of ALD HfO[sub 2] Gate Dielectrics

Authors:

Abstract
The downscaling of high- kk /metal gate transistor devices requires thin-film deposition processes that deliver not only an outstanding high- kk oxide quality, but also a strict interfacial oxide thickness control in the sub-1 nm thickness range. To study the impact of atomic layer deposition (ALD) process conditions and chemistry on the HfO2HfO2 quality and interfacial oxide thickness, we have used tetrakis[ethylmethylamino]hafnium (TEMAH) as a metal precursor and H2OH2O and O3O3 as oxidants. The deposition temperature ranged from 285 up to 365°C365°C , where TEMAH decomposition plays a role in the growth mechanism. Physical characterization and Pt dot capacitor devices have been used to study the impact of the oxidant and process conditions on the equivalent oxide thickness and gate leakage current of 2–4 nm thin HfO2HfO2 films. By combining X-ray reflectometry and ellipsometry, we evaluated the Si/high- kk interfacial oxide layer thickness. Time-of-flight secondary-ion mass spectroscopy was used to determine the C impurity levels. Both the interfacial oxide layer thickness and the C impurity level in the Si/SiO2/HfO2Si/SiO2/HfO2 stacks are strongly dependent on the oxidant. The temperature dependence of the C impurity level is opposite for O3O3 and H2OH2O . Furthermore, SiO2SiO2 regrowth was found for the O3O3 process.

This publication has 30 references indexed in Scilit: