Oriented Structure and Crystallography of Directionally Solidified LaB6—ZrB2 Eutectic
Authors:
- 21 January 1998
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 81 (1) , 237-240
Abstract
Directional solidification of LaB6—ZrB2, by use of an electron beam heating technique, yielded oriented ZrB2 fibers in a LaB6 matrix. The average diameter of the ZrB2 fibers was ∼0.2–1.2 µm, with fiber lengths up to 100 µm. Primary platelike LaB6 dendrites formed upon the solidification of an ingot with a composition of LaB6—18 wt% ZrB2. LaB6 was the first phase to nucleate when eutectic growth occurred, and ZrB2 showed nonfaceted growth. For the ingot solidified with planar growth the orientation relations of the phases were as follows: growth direction, [001]LaB6∥[00.1]ZrB2; interfacial plane, (11.0)LaB6∥(11.0)ZrB2.Keywords
This publication has 6 references indexed in Scilit:
- The structure of high-temperature solution-grown LaB6: A single-crystal diffractometry studyJournal of the Less Common Metals, 1986
- Directional Solidification of (Ti, Zr) Carbide‐(Ti, Zr) Diboride EutecticsJournal of the American Ceramic Society, 1984
- Crystallography and Microstructure of Directionally Solidified Oxide EutecticsJournal of the American Ceramic Society, 1979
- Crystallographic Properties of LaB6Formed in Molten AluminiumJapanese Journal of Applied Physics, 1975
- Single crystal growth of IVa-diborides from metal solutionsJournal of Crystal Growth, 1974
- Borides of Rare Earth MetalsJournal of the American Chemical Society, 1956