Effects of wet H 2 S containing environment on mechanical properties of NACE grade C–Mn steel pipeline girth welds
Authors:
- Tse-Ven Steven ChongTCTse-Ven Steven Chong
- Shashi Bhushan KumarSKShashi Bhushan Kumar
- Man On LaiMLMan On Lai
- Wai Lam LohWLWai Lam Loh
- 1 November 2014
- journal article
- Published by Elsevier in Engineering Fracture Mechanics
- Vol. 131, 485-503
Abstract
No abstract availableKeywords
This publication has 14 references indexed in Scilit:
- Comparison of tensile and impact behavior of carbon steel in H2S environmentsMaterials & Design (1980-2015), 2014
- Effect of hydrogen and low temperature on fatigue crack growth of pipeline steelsEngineering Fracture Mechanics, 2013
- Elastic–plastic fracture analyses for pipeline girth welds with 3D semi-elliptical surface cracks subjected to large plastic bendingInternational Journal of Pressure Vessels and Piping, 2013
- Fracture capacity of girth welded pipelines with 3D surface cracks subjected to biaxial loading conditionsInternational Journal of Pressure Vessels and Piping, 2012
- Influence of hydrogen and low temperature on mechanical behaviour of two pipeline steelsEngineering Fracture Mechanics, 2012
- Fatigue Performance of Sour Deepwater Riser Welds: Crack Growth vs. Endurance2011
- Effect of crack depth on fatigue crack growth rates for a C–Mn pipeline steel in a sour environmentInternational Journal of Fatigue, 2010
- Effects of Strain Rate on Fracture Toughness in Sour Environment2010
- Fracture Toughness Testing Using SENT Specimens in a Sour Environment2009
- Corrosion Fatigue of Welded C-Mn Steel Risers for Deepwater Applications: A State of the Art Review2005