Estimate of maximum pore size in keyhole laser welding of carbon steel
Authors:
- S. BerettaS. Beretta
- B. PrevitaliBPB. Previtali
- 1 February 2009
- journal article
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 14 (2) , 106-116
Abstract
Porosity is easily formed in welded joints during high power laser welding due to keyhole instability. Large pores have detrimental effects on the fatigue resistance of a component and cause many failures in welded parts. This paper is aimed at predicting the maximum pore dimension in long laser welded joints, starting from the sampling of large pores in shorter joints. Two sampling strategies and, consequently, two estimating techniques, both belonging to the statistics of extremes, were explored. The first approach, extreme value type, is used to estimate the size of the maximum pore in each of a series of steel samples. In each sample, the larger single pore or two large pores which are very close are the measured maximum pore. The second approach, threshold value type, is used to estimate the size of pores larger than a critical threshold in a single sample of steel. Both approaches lead to good estimates of the largest pore distribution in short laser welded joints. However, the first one is more adequate to describe the largest pore distribution, because it allows the synergetic effect of two adjacent pores to be considered. In particular, the Gumbel distribution adequately fits the experimental data even in the case of welded joints 10 times longer than the investigated bead length.Keywords
This publication has 32 references indexed in Scilit:
- Extreme value models for the assessment of steels containing multiple types of inclusionActa Materialia, 2006
- Fatigue strength of laser beam welded thin steel structures under multiaxial loadingInternational Journal of Fatigue, 2006
- A review of laser welding techniques for magnesium alloysJournal of Materials Processing Technology, 2006
- Methods for estimating the sizes of large inclusions in clean steelsActa Materialia, 2005
- Porosity reduction in Nd–YAG laser welding of stainless steel and inconel alloy by using a pulsed waveJournal of Physics D: Applied Physics, 2005
- The significance of weld imperfections and surface peening on fatigue crack propagation life of butt-welded jointsJournal of Materials Processing Technology, 2004
- Reduction of porosity content generated during Nd:YAG laser welding of A356 and AA5083 aluminium alloysMaterials Science and Engineering: A, 2003
- Interrelationship between statistical methods for estimating the size of the maximum inclusion in clean steelsActa Materialia, 2003
- The precision of methods using the statistics of extremes for the estimation of the maximum size of inclusions in clean steelsActa Materialia, 2000
- STATISTICAL ANALYSIS OF DEFECTS FOR FATIGUE STRENGTH PREDICTION AND QUALITY CONTROL OF MATERIALSFatigue & Fracture of Engineering Materials & Structures, 1998