Fatigue crack formation in bicrystals of lead
Author:
- 1 October 1966
- journal article
- research article
- Published by Taylor & Francis in Philosophical Magazine
- Vol. 14 (131) , 1019-1029
Abstract
Bicrystals of lead were fatigued in reverse bending in air and in vacuum (air pressure ∽10−6 torr) at 22°c (0·5 T m). In the first 10% of the life the boundaries became serrated by reciprocal migration and intense slip striations grew from the corners of serrations. The slip striations suggested that grain-boundary sliding was taking place during fatigue. In the presence of air, cracks first formed along the serrated boundaries and then propagated into the adjoining crystals along the slip striations emanating from the boundaries. In vacuum, grain-boundary failure was not nearly so common as in the bicrystals tested in air and ultimate failure resulted from slip-band cracking in each crystal before extensive intercrystalline cracking could develop.Keywords
This publication has 8 references indexed in Scilit:
- The effect of cycle frequency and atmospheric corrosion on the fatigue of leadPhilosophical Magazine, 1964
- Dislocation arrangements during cyclic loading of pure ironCzechoslovak Journal of Physics, 1964
- A controlled atmosphere fatigue machineJournal of Scientific Instruments, 1964
- The effect of atmosphere on the fatigue of leadActa Metallurgica, 1964
- Void Formation in Aluminum Bicrystals Subjected to Cyclic Reversed BendingCanadian Metallurgical Quarterly, 1963
- Single, Temperature-Dependent Stress-Strain Law for the Dynamic Plastic Deformation of Annealed Face-Centered Cubic MetalsJournal of Applied Physics, 1963
- The distribution of deformation in lead fatiguedin vacuoPhilosophical Magazine, 1961
- The specific energy of crystal boundaries in tinProceedings of the Royal Society of London. A. Mathematical and Physical Sciences, 1950