Corrosion of SiC Mateials in N 2 –H 2 –CO Gaseous Environments: II, Durability and Mechanical Properties
Authors:
- 1 December 1992
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 75 (12) , 3268-3277
Abstract
Three SiC materials were exposed to two gas compositions in the N 2 –H 2 –CO system at 1200° and 1300°C, 133 Pa and 98.7 kPa for 50–1000 h. The durability was evaluated by fracturing bend bars at room temperature and C‐rings at room temperature and 1300°C in argon. Fractography was used to correlate changes in strength with changes in flaw populations. In all three materials, surface pitting was the primary cause of degradation. Under some conditions it was found that flaw healing and new flaw formation occurred simultaneously. C‐rings cut from tubes did not lose strength, although pitting occurred; however, machined bend bars lost strength under identical conditions. In the case of bend bars, following an initial loss of strength (∼10%–50%) after 50–150 h, there was typically no further loss observed with increased exposure time. Due to its higher P co , degradation in an endothermic gas was generally more severe than that in a nitrogen–based gas.Keywords
This publication has 13 references indexed in Scilit:
- Corrosion of Sic Materials in N 2 –H 2 –CO Gaseous Environments: I, Thermodynamics and Kinetics of ReactionsJournal of the American Ceramic Society, 1992
- High Temperature Tube Burst Test ApparatusJournal of Testing and Evaluation, 1992
- Prediction of the Strength of Ceramic Tubular Components: Part I—AnalysisJournal of Testing and Evaluation, 1991
- Prediction of the Strength of Ceramic Tubular Components: Part II—Experimental VerificationJournal of Testing and Evaluation, 1991
- Etching of Silicon Carbide Materials at Elevated Temperatures in a Nitrogen‐Based GasJournal of the American Ceramic Society, 1991
- Experimental and Analytical Evaluation of the Mechanical Performance of a Gas-Fired Ceramic Radiant Tube at Steady-StateJournal of Testing and Evaluation, 1990
- Effect of hydrogen exposures on the strength of sintered alpha silicon carbideJournal of Materials Science, 1988
- Effect of High-Temperature Hydrogen Exposure on Sintered α-SiCAdvanced Ceramic Materials, 1988
- Effects of Hydrogen on the Microstructure and Stability of a Structural SiCAdvanced Ceramic Materials, 1988
- Fracture strength characterization of tubular ceramic materials using a simple c-ring geometryJournal of Materials Science, 1986