Low-temperature hydrophobic silicon wafer bonding
Authors:
- 8 December 2003
- journal article
- conference paper
- Published by AIP Publishing in Applied Physics Letters
- Vol. 83 (23) , 4767-4769
Abstract
By introducing a nanometer-scale H trapping defective silicon layer on bonding surfaces, the bonding surface energy of bonded oxide-free, HF dipped, hydrophobic silicon wafers can reach a silicon fracture surface energy of 2500 at 300 to 400 °C compared with 700 °C conventionally achieved. Adding boron atoms on bonding surfaces can reduce the surface hydrogen release temperature but would not increase the bonding energy unless a defective layer is also formed. This indicates that, in order to achieve high bonding energy, the released hydrogen must be removed from the bonding interface. Many prebonding treatments are available for low-temperature hydrophobic wafer bonding including the formation of an amorphous silicon layer by implantation, by or Ar plasma treatment, or by sputter deposition, followed by an HF dip and room temperature bonding in air. The interface amorphous layer may be recrystallized by annealing at elevated temperatures, e.g., at 450 °C for -implanted samples.
Keywords
This publication has 8 references indexed in Scilit:
- Microscopic theory of hydrogen in silicon devicesIEEE Transactions on Electron Devices, 2000
- Room-temperature bonding of lithium niobate and silicon wafers by argon-beam surface activationApplied Physics Letters, 1999
- Characterization of Si pn junctions fabricated by direct wafer bonding in ultra-high vacuumApplied Physics Letters, 1998
- Effects of B doping on hydrogen desorption from Si(001) during gas-source molecular-beam epitaxy from Si2H6 and B2H6Applied Physics Letters, 1996
- Self-propagating room-temperature silicon wafer bonding in ultrahigh vacuumApplied Physics Letters, 1995
- Silicon on insulator material technologyElectronics Letters, 1995
- Hydrophobic silicon wafer bondingApplied Physics Letters, 1994