Inverse grain size dependence of critical strain for serrated flow in a Fe–Mn–C twinning-induced plasticity steel
- 1 March 2012
- journal article
- research article
- Published by Taylor & Francis in Philosophical Magazine Letters
- Vol. 92 (3) , 145-152
Abstract
The grain size dependence of critical strain for serrations associated with dynamic strain aging has been examined in a twinning-induced plasticity steel. Tensile tests were conducted at various deformation temperatures and strain rates in a Fe–17Mn–0.6C steel (mass%) with grain sizes 3.5, 10, 23, 37, and 44 µm. In addition, the carbon concentration varied from 0.3 to 0.8 in the Fe–17Mn–xC steels with coarse grains. The critical strain for the onset of serrations was found to show an inverse grain size dependence, i.e., the critical strain increased with the decrease in grain size, the opposite of what occurs in conventional alloys.Keywords
This publication has 25 references indexed in Scilit:
- The effect of grain size and grain orientation on deformation twinning in a Fe–22wt.% Mn–0.6wt.% C TWIP steelMaterials Science and Engineering: A, 2010
- On the negative strain rate sensitivity of Hadfield steelScripta Materialia, 2008
- Tensile properties and twinning behavior of high manganese austenitic steel with fine-grained structureScripta Materialia, 2008
- Localized Deformation due to Portevin–LeChatelier Effect in 18Mn–0.6C TWIP Austenitic SteelISIJ International, 2007
- On dislocation accumulation and work hardening in Hadfield steelScripta Materialia, 2006
- The variation of dislocation density as a function of the stacking fault energy in shock-deformed FCC materialsMaterials Science and Engineering: A, 2002
- Influences of strain rate and grain size on yield and serrated flow in commercial Al-Mg alloy 5086Scripta Materialia, 1999
- A study of work hardening in austenitic FeMnC and FeMnAlC alloysActa Metallurgica et Materialia, 1992
- Grain size dependence of serrated yielding in a pressurized low carbon steelScripta Metallurgica, 1975
- Dislocation multiplication, vacancy accumulation, and the onset of jerky flow during forward and reverse 1 strain in Cu-3.2 at. % SnPhilosophical Magazine, 1967