Abstract
Because of the increase in demand for phosphate products with the depletion of phosphate reserves in the world, more attention is paid to the low-grade phosphate ores (13% P2O5) and the generated tailings. The present work consists of a detailed study of the low-grade phosphate ore (12.01% P2O5) of the Tozeur-Nefta deposit. It aims at elaborating the appropriate beneficiation process to improve the content of P2O5. The petrographic study has revealed the abundance of phosphatic (carbonate-fluorapatite-CFA) particles (sub-rounded pellets, ooliths, bone debris) coupled with carbonates (calcite, dolomite, ankerite) and silicates (quartz, illite, kaolonite) that make the (endo/exo) gangue of these ores. The microscopic observation/counting has shown that the phosphate-rich fraction (release mesh) occurs in the 71–315 μm size. Chemical analysis has demonstrated that the raw phosphate sample contains low amounts of P2O5 (12.01%) and MgO (4.95%) and high amounts of CaO (40.75%) and SiO2 (20.5%). Sizing, scrubbing-attrition, grinding and froth flotation methods were applied to the +71 μm fraction in order to separate phosphate-rich particles from their gangue. Scrubbing-attrition tests of the 71–315 μm fraction has helped to improve the P2O5 grade to 15.53%. Ball-grinding tests were used to reduce the coarse fraction +315 μm. Grounded materials were sieved to 71–315 μm and combined altogether with the scrubbed fraction to the flotation feed. Reverse-flotation tests of the phosphate-rich fraction (71–315 μm) have helped to improve the P2O5 grade to 27.13%, with a recovery rate of 92.38%.