Characterization of grooves in scratch resistance testing
Authors:
- 25 August 2008
- journal article
- research article
- Published by Wiley in Polymer Engineering & Science
- Vol. 48 (10) , 2060-2065
Abstract
For a number of polymers with different chemical structures and different properties we have determined scratch resistance and sliding wear (15 scratches along the same groove). We have measured cross section areas after scratching, namely the groove and side top‐ridge areas. Nanohardness after scratching was determined using nanoindentation testing both inside and outside the scratching and sliding wear grooves. Three modes of sliding wear are seen: plowing, cutting with debris formation, and densification. The dominating mode depends on the material and is reflected in nanohardness. In polycarbonate (PC) the nanohardness inside and outside the groove are practically the same; the indenter just plows the material aside without debris formation or densification. Thus, the old measure of wear as the weight of the debris formed is not usable for PC; grooves are present but there is no loosened material. By contrast, in brittle materials such as polystyrene there is debris formation and nanohardness inside the groove decreases after 15 scratching runs. A third type of behavior is seen in polyethylene and polypropylene, namely densification caused by scratching; as a result, nanohardness inside the groove increases after 15 passes of the indenter. POLYM. ENG. SCI., 2008. © 2008 Society of Plastics EngineersKeywords
This publication has 19 references indexed in Scilit:
- Connection between dynamic mechanical properties and sliding wear resistance of polymersMaterials Research Innovations, 2006
- Focused ion beam milling and scanning electron microscopy characterization of polymer+metal hybridsMaterials Letters, 2006
- Quantitative evaluation of indentation-induced densification in glassJournal of Materials Research, 2005
- Effects of carbon black on tribology of blends of poly(vinylidene fluoride) with irradiated and non-irradiated ultrahigh molecular weight polyethylenePolymer, 2005
- Friction and multiple scratch behavior of polymer+monomer liquid crystal systemsPolymer, 2005
- Fluoropolymer addition to an epoxy: phase inversion and tribological propertiesPolymer, 2001
- Phase structure and mechanical and adhesion properties of epoxy/silica hybridsPolymer, 2001
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsJournal of Materials Research, 1992
- A method for interpreting the data from depth-sensing indentation instrumentsJournal of Materials Research, 1986
- Metallurgical re-examination of wear modes II: adhesive and abrasiveThin Solid Films, 1985