Tensile yield in polypropylene
Authors:
- 1 June 1987
- journal article
- research article
- Published by Wiley in Polymer Engineering & Science
- Vol. 27 (11) , 823-828
Abstract
Untaxial tension tests to the yield point were performed on polypropylene as a function of temperature from 22 to 143°C at a strain rate of 2 min−1. At 22, 42, and 71°C, measurements were also made at strain rates from 0.02 to 8 min−1. Yield energy was found to be a linear function of temperature extrapolating to zero at the melting point (164°C). The ratio of thermal to mechanical energy to produce yielding is about three times smaller than for glassy polymers. The ratio of yield stress to (initial) Young's modulus is about 0.024 at room temperature and increases to 0.043 at 143°C. Yield stress is a linear function of unstrained volume.Keywords
This publication has 13 references indexed in Scilit:
- Tensile yield in polyethylenePolymer Engineering & Science, 1986
- Tensile yield in poly(4‐methyl pentene‐1)Polymer Engineering & Science, 1983
- Effect of temperature on the compressive stress‐strain properties of polystyrenePolymer Engineering & Science, 1978
- Tensile deformation of polychlorotrifluoroethylene in He, N2, Ar, O2, and CO2 environmentsPolymer, 1977
- Tensile yield energy in glassy polymersPolymer Engineering & Science, 1972
- Stress Softening and Strain Softening of Poly(Methyl Methacrylate) in Yielding under Constant LoadJournal of Applied Physics, 1968
- The modulus and yield stress of glassy poly(methyl methacrylate) at strain rates up to 103 inch/inch/secondJournal of Applied Polymer Science, 1968
- Pressure‐volume‐temperature behavior of polypropylenePolymer Engineering & Science, 1966
- On the cold-drawing of plasticsJournal of Applied Polymer Science, 1963
- Cold‐drawing of glass‐like and crystalline polymersJournal of Polymer Science, 1958