Interaction of Poly L-Lactide and Tungsten Disulfide Nanotubes Studied by In Situ X-ray Scattering during Expansion of PLLA/WS2NT Nanocomposite Tubes
Authors:
- Lison RocherLRLison Rocher
- Andrew S. YlitaloAYAndrew S. Ylitalo
- Tiziana Di LuccioTLTiziana Di Luccio
- Riccardo MisciosciaRiccardo Miscioscia
- Giovanni De FilippoGFGiovanni De Filippo
- Giuseppe PandolfiGPGiuseppe Pandolfi
- Fulvia VillaniFVFulvia Villani
- Alla ZakAlla Zak
- Gary H. MenaryGMGary H. Menary
- Alex B. LennonALAlex B. Lennon
- Julia A. KornfieldJKJulia A. Kornfield
Open Access
Abstract
In situ synchrotron X-ray scattering was used to reveal the transient microstructure of poly(L-lactide) (PLLA)/tungsten disulfide inorganic nanotubes (WS2NTs) nanocomposites. This microstructure is formed during the blow molding process (“tube expansion”) of an extruded polymer tube, an important step in the manufacturing of PLLA-based bioresorbable vascular scaffolds (BVS). A fundamental understanding of how such a microstructure develops during processing is relevant to two unmet needs in PLLA-based BVS: increasing strength to enable thinner devices and improving radiopacity to enable imaging during implantation. Here, we focus on how the flow generated during tube expansion affects the orientation of the WS2NTs and the formation of polymer crystals by comparing neat PLLA and nanocomposite tubes under different expansion conditions. Surprisingly, the WS2NTs remain oriented along the extrusion direction despite significant strain in the transverse direction while the PLLA crystals (c-axis) form along the circumferential direction of the tube. Although WS2NTs promote the nucleation of PLLA crystals in nanocomposite tubes, crystallization proceeds with largely the same orientation as in neat PLLA tubes. We suggest that the reason for the unusual independence of the orientations of the nanotubes and polymer crystals stems from the favorable interaction between PLLA and WS2NTs. This favorable interaction leads WS2NTs to disperse well in PLLA and strongly orient along the axis of the PLLA tube during extrusion. As a consequence, the nanotubes are aligned orthogonally to the circumferential stretching direction, which appears to decouple the orientations of PLLA crystals and WS2NTs.Keywords
Funding Information
- Horizon 2020 (813869, 691238)
- National Science Foundation Graduate Research Fellowship (DGE‐1745301)
This publication has 68 references indexed in Scilit:
- Rheologically Determined Critical Shear Rates for Shear-Induced Nucleation Rate Enhancements of Poly(lactic acid)ACS Sustainable Chemistry & Engineering, 2013
- Realizing the enhancement of interfacial interaction in semicrystalline polymer/filler composites via interfacial crystallizationProgress in Polymer Science, 2012
- First Serial Assessment at 6 Months and 2 Years of the Second Generation of Absorb Everolimus-Eluting Bioresorbable Vascular ScaffoldCirculation: Cardiovascular Interventions, 2012
- Surface functionalization of nanoparticles for nanomedicineChemical Society Reviews, 2012
- Stent Thrombogenicity Early in High-Risk Interventional Settings Is Driven by Stent Design and Deployment and Protected by Polymer-Drug CoatingsCirculation, 2011
- Bioresorbable ScaffoldCirculation, 2011
- Scaling Up of the WS2Nanotubes SynthesisFullerenes, Nanotubes and Carbon Nanostructures, 2010
- Polymer-Nanoparticle Composites: From Synthesis to Modern ApplicationsMaterials, 2010
- Nanocomposites of polymer and inorganic nanoparticles for optical and magnetic applicationsNano Reviews, 2010
- Influence of Topography on Endothelialization of Stents: Clues for New DesignsJournal of Long-Term Effects of Medical Implants, 2000