This paper outlines permeability and loss measurements on large uncut toroidal cores of Hipersil and Supermendur alloys. With forced cooling, large increments of core induction can be utilized; with a reset core, pulse permeability is much higher than it is in cut cores, and alters pulse transformer design radically. At inductions up to 24 kgauss, pulse permeability of fully oriented Hipersil and Supermendur alloys were about 6000, compared to approximately 1500 for cut cores at lower flux densities. It appears practicable from these tests to operate Hipersil alloy with excursions of induction up to 30 kgauss and Supermendur alloy up to 40 kgauss, and to reduce pulse transformer weight by 80%.