Relations between Piezoelectric Properties and Microstructure in Poled Piezoelectric Ceramics by Applied Uniaxial Compressive Stress
- 1 September 1991
- journal article
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 30 (9S) , 2256
Abstract
Relations among k p, f r·d, Q m and domain configurations in some piezoelectric ceramics with various Q m values were investigated under a polarization process (poling treatment) and depolarization process (applied stress treatment). In those materials, k p values in Pb(Zr0.17)(Ti0.33)(Ni1/3Nb2/3)0.5O3 ceramics (low Q m) decreased markedly with applied uniaxial compressive stress increase, and became 0.402 from 0.702 (initial k p value) by 49 MPa, while 90° and 180° domain patterns revealed by chemical etching were not changed, even by either poling or applied stress treatments. However, k p values in (Pb0.625Ca0.375)TiO3 ceramics (high Q m) decreased slightly by 49 MPa, and a clear difference in the 90° domain pattern arrangement was observed before and after both poling and applied stress treatments.Keywords
This publication has 1 reference indexed in Scilit:
- Ultrasonic Velocities in Polarized Barium Titanate CeramicsThe Journal of the Acoustical Society of America, 1955