Observation of transcrystalline growth of PLA crystals on sisal fibre bundles and the effect of crystal structure on interfacial shear strength
Authors:
- 1 February 2012
- journal article
- research article
- Published by Taylor & Francis in Composite Interfaces
- Vol. 19 (1) , 39-50
Abstract
Hot-stage microscopy was used to characterise crystal growth at the interface between sisal fibre bundles and a polylactic acid (PLA) matrix in order to better understand the mechanical properties of sisal fibre–PLA composites. Cooling rates and crystallisation temperatures and times were varied to influence crystalline morphology at the interface. Single sisal fibre bundles were evaluated in their as received state or treated with 6 wt.% caustic soda solution for 48 h at room temperature. A microbond shear test was used to characterise the shear strength of the interface as a function of fibre surface treatment. These tests were performed on sisal fibre bundles carefully embedded in flat films of PLA supported on card mounts. Fibre bundles in a PLA matrix were cooled from 180 °C at rates from 2 to 9 °C/min and then crystallised isothermally. For as received fibre bundles uneven growth of PLA spherulites occurred at all cooling rates and crystallisation temperatures. For caustic soda treated fibres, uneven spherulitic growth was observed at crystallisation temperatures at and above 125 °C. In contrast, transcrystalline growth was observed for samples cooled to 120 °C at cooling rates from 2 to 6 °C/min and then allowed to crystallise. The microbond shear strengths of untreated and caustic soda treated fibre bundles were evaluated using Weibull statistics and the caustic soda treated fibres exhibited higher interfacial shear strengths in comparison to untreated fibres, reflecting the development of a transcrystalline layer at the fibre to matrix interface.Keywords
This publication has 13 references indexed in Scilit:
- The structure of cotton and other plant fibres2009
- A novel processing technique for thermoplastic manufacturing of unidirectional composites reinforced with jute yarnsComposites Part A: Applied Science and Manufacturing, 2006
- Mechanical properties of alkali treated plant fibres and their potential as reinforcement materials II. Sisal fibresJournal of Materials Science, 2006
- Properties of lactic acid based polymers and their correlation with compositionProgress in Polymer Science, 2002
- Chemical modification of hemp, sisal, jute, and kapok fibers by alkalizationJournal of Applied Polymer Science, 2002
- A study of transcrystallinity and its effect on the interface in flax fibre reinforced composite materialsComposites Part A: Applied Science and Manufacturing, 2001
- Crystallization behaviour of poly(l-lactide)Polymer, 1998
- Transcrystallinity effects in thin polymer films. Experimental and theoretical approachColloid and Polymer Science, 1994
- Surface induced crystallization in ultrahigh-modulus polyethylene fiber-reinforced polyethylene compositesMacromolecules, 1991
- Transcrystallinity in polypropyleneJournal of Polymer Science: Polymer Chemistry Edition, 1984