Investigation on the fatigue life characteristic of kenaf/glass woven-ply reinforced metal sandwich materials
- 8 September 2017
- journal article
- research article
- Published by SAGE Publications in Journal of Sandwich Structures & Materials
- Vol. 21 (7) , 2440-2455
Abstract
Fatigue life characteristic of hybrid composite reinforced metal laminate is a notable investigation since this kind of material offers several superior characteristics over conventional metallic alloy. A majority of the researches have focused on the mechanical properties of hybrid composite and conventional fibre metal laminate such as glass reinforced aluminium epoxy and aramid fibre reinforced aluminium laminate. However, investigation on the fatigue life behaviour of hybrid composite reinforced metal laminate still remains unexplored. In this study, the fatigue life characteristic of hybrid kenaf/glass reinforced metal laminate with different fibre configurations, orientation and stress ratio was presented. Fibre metal laminate was manufactured through hot press moulding compression method using annealed aluminium 5052 as the skin layers and the composite laminate as the core constituent. Tensile test was conducted at a quasi-static rate in accordance with ASTM E8 while tension–tension fatigue test was conducted at force controlled constant amplitude according to ASTM E466. Experimental results revealed that fibre metal laminate with 0°/90° fibre orientation exhibited better tensile and fatigue properties compared to fibre metal laminate with ±45° fibre orientation regardless of the woven-ply fibre configurations. Besides that, it was identified that higher stress ratio improves the fatigue life cycle of the fibre metal laminate structures.Keywords
This publication has 19 references indexed in Scilit:
- Partial Replacement of Glass Fiber by Woven Kenaf in Hybrid Composites and its Effect on Monotonic and Fatigue PropertiesBioResources, 2015
- Tension–tension fatigue behaviour of woven flax/epoxy compositesJournal of Reinforced Plastics and Composites, 2015
- Impact resistance of fiber-metal laminates: A reviewInternational Journal of Impact Engineering, 2012
- Impact and fatigue properties of hemp–glass fiber hybrid biocompositesJournal of Reinforced Plastics and Composites, 2011
- Mechanical performance of Kraft fibre reinforced polypropylene composites: Influence of fibre length, fibre beating and hygrothermal ageingComposites Part A: Applied Science and Manufacturing, 2008
- The prediction of tensile failure in titanium-based thermoplastic fibre–metal laminatesComposites Science and Technology, 2006
- The influence of fibre length and concentration on the properties of glass fibre reinforced polypropylene. 6. The properties of injection moulded long fibre PP at high fibre contentComposites Part A: Applied Science and Manufacturing, 2005
- The high velocity impact response of composite and FML-reinforced sandwich structuresComposites Science and Technology, 2004
- Fiber metal laminates: An advanced material for future aircraftJournal of Materials Processing Technology, 1997
- Fracture of glass/polypropylene laminates: influence of cooling rate after mouldingComposites, 1994