Abnormal grain growth in sintered Nd-Fe-B magnets
Authors:
- 1 May 1990
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 67 (9) , 4629-4631
Abstract
Abnormal grain growth was found in sintered Nd-Fe-B magnets which are made from powder milled after hydrogen decrepitation. The abnormal grain size in the magnets sintered at 1000 °C for 1.5 h was as large as 400 μm. The formation of abnormally large grains reduced the magnetic properties. As sintering temperature increased, the number of large grains increased and coercivity reduced. However, abnormal grain growth was rarely found when the magnets were fabricated without hydrogen decrepitation. A grain growth mechanism is discussed in relation to the effect of hydrogenation and sintering process.Keywords
This publication has 8 references indexed in Scilit:
- The influence of sintering aids on the texture and remanence of Nd-Fe-B magnet alloysJournal of Magnetism and Magnetic Materials, 1989
- Magnetization reversal in nucleation controlled magnets. II. Effect of grain size and size distribution on intrinsic coercivity of Fe-Nd-B magnetsJournal of Applied Physics, 1988
- Magnetization reversal in nucleation controlled magnets. I. TheoryJournal of Applied Physics, 1988
- Effect of oxygen on magnetic properties of Nd-Fe-B magnetsJournal of Applied Physics, 1988
- A texture study of anisotropic sintered Nd-Fe-B magnetsJournal of Applied Physics, 1988
- The production of a Nd-Fe-B permanent magnet by a hydrogen decrepitation/attritor milling routeJournal of Materials Science, 1986
- The metallurgy of the iron-neodymium-boron permanent magnet systemMaterials Letters, 1984
- New material for permanent magnets on a base of Nd and Fe (invited)Journal of Applied Physics, 1984