Post-processing Methods to Improve Strength of Particle-Bed 3D Printed Geopolymer for Digital Construction Applications
Open Access
- 4 July 2019
- journal article
- research article
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 6
Abstract
The strength of powder-based 3D printed geopolymer samples immediately after the de-powdering process (“green” strength) is inherently very low. Therefore, different post-processing techniques have been explored in the previous study of the authors to enhance the “green” strength of the printed geopolymer. The highest strength of around 30 MPa was achieved for the printed slag-based geopolymer sample cured in an alkaline solution for 7 days at 60°C. Although this strength is sufficient for a wide range of construction applications, the necessity for the heat curing procedure, which requires a significant amount of energy, can compromise the sustainability credentials of the developed powder-based 3D printed geopolymer and limit its commercial viability and large-scale applications in the construction industry. To tackle this issue, this study aims to develop a new post-processing method which eliminates the necessity for the heat curing. The influences of type of curing medium, duration and temperature of curing, and testing direction on the compressive strength of the printed geopolymer were investigated. The “green” printed geopolymer samples were immersed in four different curing mediums, including two sodium (Na)-based, and two potassium (K)-based activators with different alkali modulus (SiO2/M2O where M = Na or K), and cured at two different curing temperatures (ambient temperature (23°C) vs. 60°C) for 7 and 28 days. The compressive strength of the “post-processed” printed geopolymer specimens was measured in two different testing directions, namely the binder jetting direction and layer stacking direction. The results showed that the 28-day compressive strength of the ambient temperature cured printed geopolymer sample was comparable to the 7-day compressive strength of the corresponding heat cured sample. Therefore, the feasibility of enhancing the strength of printed geopolymer by curing in an alkaline solution at ambient temperature was established. This developed post-processing method based on the ambient temperature curing is more viable and less energy-intensive, yet provides comparable strength, as compared to the previously developed post-processing method based on the heat curing. The results also showed that the strength of the printed geopolymer samples cured in the K-based activators was lower than that of the specimens cured in the Na-based activators.Keywords
This publication has 42 references indexed in Scilit:
- Vision of 3D printing with concrete — Technical, economic and environmental potentialsCement and Concrete Research, 2018
- Cements in the 21st century: Challenges, perspectives, and opportunitiesJournal of the American Ceramic Society, 2017
- Structure, Properties, and In Vitro Behavior of Heat-Treated Calcium Sulfate Scaffolds Fabricated by 3D PrintingPLOS ONE, 2016
- An exploration of binder jetting of copperRapid Prototyping Journal, 2015
- Building components for an outpost on the Lunar soil by means of a novel 3D printing technologyActa Astronautica, 2014
- Two-phase geopolymerization of kaolinite-based geopolymersApplied Clay Science, 2013
- Application of Calcium Phosphate Materials in DentistryInternational Journal of Biomaterials, 2013
- The role of inorganic polymer technology in the development of ‘green concrete’Cement and Concrete Research, 2007
- Geopolymer technology: the current state of the artJournal of Materials Science, 2006
- Alkali activated fly ash binders. A comparative study between sodium and potassium activatorsMateriales de Construcción, 2006