Characterization of Silk/Poly 3-Hydroxybutyrate-chitosan-multi-walled Carbon Nanotube Micro-nano Scaffold: A New Hybrid Scaffold for Tissue Engineering Applications
Open Access
- 1 January 2018
- journal article
- research article
- Published by Medknow in Journal of Medical Signals & Sensors
- Vol. 8 (1) , 46-52
Abstract
Background: Long-term healing tissue engineering scaffolds must hold its full mechanical strength at least for 12 weeks. Nano-micro scaffolds consist of electrospinning nanofibers and textile microfibers to support cell behavior and mechanical strength, respectively. Methods: The new nano-micro hybrid scaffold was fabricated by electrospinning poly 3-hydroxybutyrate-chitosan-multi-walled carbon nanotube (MWNT functionalized by COOH) solution on knitted silk in a random manner with different amounts of MWNT. The physical, mechanical, and biodegradation properties were assessed through scanning electron microscopy, Fourier-transform infrared (FTIR) spectroscopy, water contact angle test, tensile strength test, and weight loss test. The scaffold without MWNT was chosen as control sample. Results: An increase in the amount of MWNT up to 1 wt% leads to better fiber diameter distribution, more hydrophilicity, biodegradation rate, and higher tensile strength in comparison with other samples. The porosity percentage of all scaffolds is more than 80%. According to FTIR spectra, the nanofibrous coat on knitted silk did not have any effect on silk fibroin crystallinity structures, and according to tensile strength test, the coat had a significant effect on tensile strength in comparison with pure knitted silk (P ≤ 0.05). The average fiber diameter decreased due to an increase in electrical conductivity of the solution and fiber stretch in electrical field due to MWNTs. The scaffold containing 1 wt% MWNT was more hydrophilic due to the presence of many COOH groups of functionalized MWNT, thus an increase in the hydrolysis and degradation rate of this sample. Conclusions: High intrinsic tensile strength of MWNTs and improvement of nano-micro interface connection lead to an increase in tensile strength in scaffolds containing MWNT.Keywords
This publication has 15 references indexed in Scilit:
- Polysaccharide-based nanocomposites and their applicationsCarbohydrate Research, 2015
- In vitro study on silk fibroin textile structure for Anterior Cruciate Ligament regenerationMaterials Science and Engineering: C, 2013
- Fabrication and characterization of regenerated silk scaffolds reinforced with natural silk fibers for bone tissue engineeringJournal of Biomedical Materials Research Part A, 2013
- PLGA nanofiber‐coated silk microfibrous scaffold for connective tissue engineeringJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2010
- Optimization of the silk scaffold sericin removal process for retention of silk fibroin protein structure and mechanical propertiesBiomedical Materials, 2010
- Phase separation, pore structure, and properties of nanofibrous gelatin scaffoldsBiomaterials, 2009
- Preparation of chitosan–gelatin hybrid scaffolds with well-organized microstructures for hepatic tissue engineeringActa Biomaterialia, 2009
- Development of hybrid polymer scaffolds for potential applications in ligament and tendon tissue engineeringBiomedical Materials, 2007
- Silk as a biomaterialProgress in Polymer Science, 2007
- Nano- and micro-fiber combined scaffolds: A new architecture for bone tissue engineeringJournal of Materials Science: Materials in Medicine, 2005