Radio frequency plasma chemical vapor deposited thin films of diamond-like carbon/SiO[sub 2] nanocomposites by way of tetraethoxysilane
Authors:
- Jay J. SenkevichJSJay J. Senkevich
- Donald E. LeberDLDonald E. Leber
- Michael J. TutorMTMichael J. Tutor
- Noel A. HeiksNHNoel A. Heiks
- Greg A. Ten EyckGEGreg A. Ten Eyck
- David W. ScherrerDSDavid W. Scherrer
- Yong Tae KimYKYong Tae Kim
- Suk‐Ki MinSMSuk‐Ki Min
- Jong Sung HongJHJong Sung Hong
- Choong Ki KimCKChoong Ki Kim
- M. L. HammondMHM. L. Hammond
- Kunio OkimuraKOKunio Okimura
- 1 January 1999
- journal article
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B
- Vol. 17 (5) , 2129
Abstract
Diamond-like carbon (DLC) has gained recent interest since it can be easily deposited at room temperature with a conventional radio frequency (rf) plasma. DLC has the potential benefits of a low coefficient friction, high hardness, and can be deposited with common inexpensive precursors. However, for optical applications used in the visible spectrum DLC has the problem of having a peak absorbance at 305–330 nm. This absorbance with thicker films or for higher volume fractions of DLC in a nanocomposite structure monotonically decreases into the visible spectrum where the film appears yellowish to brownish. The work here has focused on using a common alkoxy silane precursor, tetraethoxysilane, to deposit nanocomposites at room temperature using an ion-assisted process to deposit transparent antiscratch films in the visible spectrum. The highest scratch resistant nonabsorbing films were deposited at low pressures (∼15 mTorr), high flows of oxygen (>120 sccm), at modest power densities (∼0.2 W/cm2), and low flows of argon (15 sccm) keeping the TEOS bubbler temperature constant. Under these conditions very little carbon is deposited, hence, little absorption. However, more important argon bombardment allows the to be nearly hydroxyl free and the carbon that is left may allow the films to retain a lower coefficient of friction and their hydrophobicity. At higher system pressures (∼200 mTorr) the films deposited were much softer than the films deposited at lower system pressures (∼30 mTorr), hence, the importance of ion bombardment. At higher power densities (∼1.4 W/cm2) DLC is deposited independent of other system parameters. The measured absorbtivity of DLC was 31 600 cm−1 at 305–330 nm.
Keywords
This publication has 18 references indexed in Scilit:
- Diamond-like nanocomposite coatings for low-wear and low-friction applications in humid environmentsThin Solid Films, 1998
- Diamond-like nanocomposite coatings (a-C:H/a-Si:O) for tribological applicationsDiamond and Related Materials, 1998
- Structural dependence of mechanical properties of Si incorporated diamond-like carbon films deposited by RF plasma-assisted chemical vapour depositionThin Solid Films, 1997
- Room Temperature Deposition of Silicon Dioxide Films by Ion‐Assisted Plasma Enhanced Chemical Vapor DepositionJournal of the Electrochemical Society, 1996
- A Study on the Residual Stress of Diamond-Like Carbon Films Deposited by Magnetically Enhanced RF PECVDMRS Proceedings, 1996
- Deposition of diamond-like carbon film in CH4He r.f. plasmaDiamond and Related Materials, 1995
- Scanning tunneling microscopy of diamond-like nanocomposite filmsApplied Physics Letters, 1994
- Diamond-like carbon thin films prepared by rf-plasma CVD1991
- Diamond-like carbon films prepared by rf plasma depositionVacuum, 1990
- Surface and Colloid Science1979