Abstract
The objective of the present study was to evaluate the effect of different surface treatments and polymerization protocols on the bond strength of brackets to enamel, and the degree of conversion of the bonding agents. 120 bovine crowns were embedded in acrylic resin blocks and sanded. Next, the blocks were randomly assigned into 12 groups. Metal brackets were bonded to enamel according to the “surface treatment” factor (A: Phosphoric Acid; ATxt: Phosphoric Acid + Transbond XT Primer®; Tse: Transbond Plus Self Etching Primer®; and SBU: Scotchbond Universal®) and “polymerization” factor (R20: Radii-Cal®/20 seconds; V20: Valo Cordless®/20 seconds; and V3: Valo Cordless®/3 seconds). All samples were stored for 6 months (water, 37ºC) and then subjected to a shear bond strength test (SBS). Bond failures were classified according to the Adhesive Remnant Index (ARI) and analyzed with the Kruskal-Wallis and Mann-Whitney tests (5%). Using the same factors, 120 resin discs were made to assess the degree of conversion (DC) of the monomer. Data from the SBS (MPa) and DC (%) were analyzed by analysis of variance (2 factors) and Tukey’s test (5%). For the SBS, the factors “polymerization” (R20 = 8.1B; V20 = 13.2A; V3 = 5.2C, p = 0.0001) and “surface treatment” (A = 3.1C; ATxt = 13.6A; Tse = 12.3A; SBU = 6.3B, p = 0.0001) were statistically significant among groups. The highest adhesion value were found for the ATxt/V20 group (22.2A) and the lowest value for the A/R20 group (1.2E). Regarding ARI, score 2 was the most prevalent in groups A, ATxt, V20 and V3, while score 4 was the most prevalent in the Tse, SBU and R20 groups, with no significant difference between them (p = 1.0). Regarding DC, the factors “polymerization” (R20 = 66.6A; V20 = 58.4B; V3 = 45.1C, p = 0.0001) and “surface treatment” (A = 52B, ATxt = 59.7A, Tse = 51.4B, SBU = 63.8A, p = 0.0001) were statistically significant. Tse was more sensitive to the variations in polymerization protocols than the other surface treatments. Treatment A did not present suitable bond strength or degree of conversion.Keywords
This publication has 37 references indexed in Scilit:
- Comparison of the superelasticity of different nickel–titanium orthodontic archwires and the loss of their properties by heat treatmentJournal of Materials Science: Materials in Medicine, 2016
- Comparing orthodontic bond failures of light-cured composite resin with chemical-cured composite resin: A 12-month clinical trialAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2016
- Evolution of imaging and management systems in orthodonticsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2016
- In-vitro bond strengths and clinical failure rates of metal brackets bonded with different light-emitting diode units and curing timesAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2016
- Orthodontic bonding with and without primer: a randomized controlled trialEuropean Journal of Orthodontics, 2015
- Comparative assessment of alignment efficiency and space closure of active and passive self-ligating vs conventional appliances in adolescents: A single-center randomized controlled trialAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2014
- Shear bond strength comparison of moisture-insensitive primer and self-etching primerJournal of Orthodontic Science, 2014
- Antibacterial Activity of Various Self-etching Adhesive Systems Against Oral StreptococciOperative Dentistry, 2010
- Clinical Study of Temporary Anchorage Devices for Orthodontic TreatmentThe Bulletin of Tokyo Dental College, 2010
- A Simple Method of Increasing the Adhesion of Acrylic Filling Materials to Enamel SurfacesJournal of Dental Research, 1955