Abstract
Ordered-hexagonal silica materials such as MCM41 and SBA15 have important applications in heterogeneous catalysis and biomass conversion due to their chemical stability and mesoporous structure. Low-temperature grafting (LG) is one of the most common functionalization methods to modify the silica surface with acidic/basic or hydrophobic/hydrophilic moieties. However, the materials prepared by this method are prone to the leaching of functional groups into the reaction medium. The exact nature of the leaching phenomenon has not been fully addressed in the literature. In this contribution, we have investigated this process at the molecular level by combining well-controlled reaction experiments and several characterization techniques (FT-IR, 1H-29Si CPMAS NMR, XRD, TGA and BET). We have found that leaching is originated by the presence of terminal surface silanols, which render the catalysts susceptible to the attack of water and polar compounds. Hence, leaching can be better described as a partial dissolution of the surface layers of the silica, thus removing the functional groups during this process. Therefore, an effective strategy to minimize leaching is to reduce the density of free silanols via full functionalization of the surface. We propose a novel silylation method, high-temperature grafting, which allows the grafting process to be conducted at high temperatures (180oC) under solvent-free conditions. By this method, a more complete silylation of surface silanols is obtained. Consequently, the samples prepared by this high-temperature grafting (HG) method are highly stable during acid-catalyzed alkylation reaction, conducted under severe conditions (high temperature and in the presence of polar solvents).
Funding Information
  • Basic Energy Sciences (DE-SC0018284)

This publication has 70 references indexed in Scilit: