Enhanced Corrosion-Resistant Stainless Steel OCTG of 17Cr for Sweet and Sour Environments

Authors:

Abstract
Enhanced corrosion-resistant 17Cr stainless OCTG (17Cr-4Ni-2.5Mo-1Cu-1W-lowC) is discussed in terms of sweet and sweet-sour environments in comparison with martensitic stainless UNS No.S42000 (13Cr-0.20C), modified-13Cr (13Cr-5Ni-2Mo-lowC), UNS No.S42625 (15Cr-6Ni-2Mo-1Cu-lowC) and duplex stainless UNS No.S31803 (22Cr-5Ni-3Mo-N-lowC) or UNS No.S31260 (25Cr-6Ni-3Mo-N-lowC). Especially in CO2 corrosion, the application limit temperature is 230 °C (450 °F) for 17Cr, which shows the highest temperature compared with 130 °C (270 °F) for UNS No.S42000, 165 °C (330 °F) for modified-13Cr, 200 °C (390 °F) for UNS No.S42625. Other corrosion data for 17Cr, such as SSC and pitting resistance, also shows better corrosion-resistant characteristics than any other martensitic stainless OCTGs of UNS No.S42000, modified-13Cr, UNS No.S42625. In addition, the microstructure of 17Cr is composed mainly of martensite and ferrite with a small amount of austenite. Therefore, 17Cr as well as martensitic stainless steel OCTGs have high-strength at room temperature without requiring any cold-working-based strengthening needed in austenite-ferrite UNS No.S31803 or UNS No.S31260, and also keep high-temperature-strength even at 100 to 250 °C (212 to 482 °F), while duplex UNS No.S31803 and UNS No.S31260 sharply drop in high-temperature-strength due to the release of their cold-working-based strains