Chemical Composition, Knoop Hardness, Surface Roughness, and Adhesion Aspects of Additively Manufactured Dental Interim Materials
- 8 December 2020
- journal article
- research article
- Published by Wiley in Journal of Prosthodontics
- Vol. 30 (8) , 698-705
Abstract
Purpose: To measure the chemical composition, Knoop hardness, surface roughness, and composite bond strength of additive manufactured (AM) and conventional interim materials.Material and Methods: Disks were prepared using conventionally (CNV group) and additively manufactured (AM group) materials: CNV‐1 (Protemp 4; 3M ESPE), CNV‐2 (Anaxdent new outline dentin; Anaxdent), AM‐1 (FreePrint temp; Detax), AM‐2 (E‐Dent 400 C&B MFH; Envisiontec), AM‐3 (NextDent C&B MFH; 3D Systems), and AM‐4 (Med620 VEROGlaze; Stratasys). Each group was subdivided into 3 subgroups (n = 20) for analyzing Knoop hardness (KHN), chemical composition, superficial roughness (Ra), and composite shear bond strength. The first subgroup was exposed to a microhardness test. Subsequently, EDAX analysis was selected to analyze the chemical composition. The second subgroup was selected to measure the superficial roughness (Ra) using a contact profilometer. The third subgroup was used to measured composite shear bond strength using a universal testing apparatus. A digital microscope was used to analyze the fracture mode. The Shapiro‐Wilk test showed normally distributed data. One‐way ANOVA and post hoc Sidak tests were selected (α = 0.05).Results: Major variances in chemical composition were observed among the specimens. Significant differences in Knoop hardness (p < 0.001) and surface roughness (p < 0.001) were detected. The AM‐4 (13.45 ± 2.93 KHN), the CNV‐2 (13.35 ± 5.84 KHN), the AM‐2 (13.03 ± 3.29 KHN), and the AM‐1 (12.55 ± 2.93 KHN) groups obtained the highest Knoop hardness values, followed by the AM‐3 and the CNV‐1 groups (p < 0.05). The AM‐1 group (1.88 ± 1.11 Ra) obtained the highest surface roughness values among the groups, followed by the AM‐3 group (0.90 ± 0.14 Ra) (p < 0.05). However, no significant differences in shear bond strength values were found between the groups ranging from 23.18 ± 8.88 MPa to 33.29 ± 9.17 MPa (p = 0.061). All the groups showed a cohesive mode of failure.Conclusions: The AM interim materials tested had significant chemical composition variations compared to conventional materials. For the mechanical properties evaluated, the AM materials obtained appropriate mechanical properties for use as an interim dental restoration. However, further studies are required to evaluate more extensively its mechanical properties and verify their applicability in the oral cavity, clinical behavior, and biocompatibility.Keywords
This publication has 34 references indexed in Scilit:
- Fracture toughness of cross-linked and non-cross-linked temporary crown and fixed partial denture materialsDental Materials, 2009
- Influence of surface treatments on the bond strength of repaired resin composite restorative materialsDental Materials, 2009
- Shear Bond Strength of Provisional Restoration Materials Repaired with Light-cured ResinsOperative Dentistry, 2008
- Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditionsDental Materials, 2007
- Effect of Intermediate Agents and Pre-heating of Repairing Resin on Composite-repair BondsOperative Dentistry, 2007
- Repair of bis-acryl provisional restorations using flowable composite resinThe Journal of Prosthetic Dentistry, 2004
- Effect of combinations of surface treatments and bonding agents on the bond strength of repaired compositesThe Journal of Prosthetic Dentistry, 1997
- Build-up and Repair of Light-cured Composites: Bond StrengthJournal of Dental Research, 1984
- Unreacted Methacrylate Groups on the Surfaces of Composite ResinsJournal of Dental Research, 1982
- The provisional fixed partial dentureThe Journal of Prosthetic Dentistry, 1975