Abstract
Nanocrystalline zirconia with a grain size of ∼5 nm was surface‐doped with 3 and 30 mol% alumina by chemical vapor synthesis using two sequential hot‐wall reactors. The powders were characterized by high‐resolution transmission electron microscopy, X‐ray diffractometry (XRD), and nitrogen adsorption. Aqueous dispersions were studied by zeta‐potential measurements and photocorrelation spectroscopy. Green and sintered ceramic bodies were investigated by high‐resolution scanning electron microscopy, XRD, and nitrogen adsorption. Zirconia surface‐doped with 3 mol% of alumina displays substantial changes in dispersability and sinterability compared with pure nanocrystalline zirconia.