Finite element analysis of the mechanical behaviour of insulated rail joints due to impact loadings
- 7 December 2014
- journal article
- research article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part F: Journal of Rail and Rapid Transit
- Vol. 230 (3) , 759-773
Abstract
Insulated rail joints (IRJs) are safety-critical components in the signalling system of rail corridors. They are subjected to dynamic loads generated by heavy rolling-stock/track- system interactions and degrade faster than the other components of the rail track. Degraded IRJs diminish the reliability of the signalling system, thus posing a serious threat to the safety of rail operations. Therefore, there is a pressing need to closely examine the failure mechanisms of the end posts made of insulated material and inserted into the discontinuity in the rail at IRJs with a view to improving their service life, reliability and efficiency. Only a limited literature is available that examines different materials for IRJ end posts, and these primarily focus on contact pressure and contact stress distributions in the vicinity of the end post, disregarding the damage to the rail ends and end post materials. In this paper, a detailed three-dimensional finite element analysis procedure is carried out to quantify plastic deformation and material damage to the end post and railhead materials of IRJs due to a wheel load above that of the shakedown limit of rail steel. A modified Hertzian contact pressure distribution is considered in this simulation. A 5 mm thickness of an end post is considered at the discontinuity in the rail, which is required to form the six-bolt IRJ. Three popular IRJ end post materials are considered in this study: fibreglass, polyhexamethylene adipamide, and polytetrafluoroethylene. A total of 2000 cycles of a 174 kN dynamic wheel load (in pressure format over the wheel/rail contact patch) are applied on the top of the rail’s surface in the vicinity of the IRJ. Equivalent plastic deformations along with vertical and longitudinal plastic strains for unloaded conditions are presented. The strain plots depict damage of end post materials and ratchetting failure of rail ends. The ratchetting failure modes follow the established trend of decay in ratchetting rate in successive wheel load cycles. Comparisons of strain and stress on the railhead surface and in the railhead sub-surface considering all three different end post materials are put forward. Out of the three end post materials, fibreglass is the optimal material considering the ratchetting mode for the damage of the railhead material.Keywords
This publication has 13 references indexed in Scilit:
- On the low cycle fatigue failure of insulated rail joints (IRJs)Engineering Failure Analysis, 2014
- Sub-modelling for the ratchetting failure of insulated rail jointsInternational Journal of Mechanical Sciences, 2013
- Experimental Investigation of Wheel/Rail Rolling Contact at Railhead EdgeExperimental Mechanics, 2012
- Dynamic vehicle–track interaction and plastic deformation of rail at rail weldsEngineering Failure Analysis, 2009
- Flexural behaviour of bonded-bolted butt joints due to bolt loosenessAdvances in Engineering Software, 2006
- Prediction of dynamic train–track interaction and subsequent material deterioration in the presence of insulated rail jointsVehicle System Dynamics, 2006
- Contact-impact stress analysis of rail joint region using the dynamic finite element methodWear, 2005
- Cyclic ratchetting and failure of a pearlitic rail steelFatigue & Fracture of Engineering Materials & Structures, 2000
- Analysis and tests of boned insulted rail joints subjected to vertical wheel loadsInternational Journal of Mechanical Sciences, 1999
- Shakedown, Residual Stress and Plastic Flow in Repeated Wheel-Rail Contact1993