Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate
Authors:
- Michael JendrasMJMichael Jendras
- Lothar BorchersLBLothar Borchers
- Friedrich-Wilhelm BachFBFriedrich-Wilhelm Bach
- Meike StieschMSMeike Stiesch
- Philipp KohorstPKPhilipp Kohorst
- 1 April 2012
- journal article
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 56 (2) , 93-101
Abstract
The aim of this study was to assess the effect of differences in the thermal expansion behaviour of veneering ceramics on the adhesion to Y-TZP, using a fracture mechanics approach. Seven veneering ceramics (VM7, VM9, VM13, Lava Ceram, Zirox, Triceram, Allux) and one Y-TZP ceramic were investigated. Thermal expansion coefficients and glass transition temperatures were determined to calculate residual stresses (σ(R), MPa) between core and veneer. Subsequently, the veneering ceramics were fired onto rectangular shaped zirconia specimens, ground flat and notched on the veneering porcelain side. Then specimens were loaded in a four-point bending test and load-displacement curves were recorded. The critical load to induce stable crack extension at the adhesion interface was evaluated to calculate the strain energy release rate (G, J/m(2)) for each system. Residual stresses ranged from -48.3±1.5MPa (VM7) to 36.1±4.8MPa (VM13) with significant differences between all groups (p<0.05). The strain energy release rate of the Y-TZP/veneer specimens ranged from 8.2±1.7J/m(2) (Lava Ceram) to 17.1±2.8J/m(2) (VM9). Values for G could not be obtained with the VM7, Allux and VM13 specimens, due to spontaneous debonding or unstable crack growth. Except for Triceram and Zirox specimens, strain energy release rate was significantly different between all groups (p<0.05). Thermal residual stresses and strain energy release rates were correlated. Slight compressive stresses in the region of -20MPa were beneficial for the Y-TZP/veneer interfacial adhesion. Stresses higher or lower than this value exhibited decreased adhesion.Keywords
This publication has 29 references indexed in Scilit:
- Influence of cooling rate on zirconia/veneer interfacial adhesionActa Biomaterialia, 2010
- Thermal compatibility of dental ceramic systems using cylindrical and spherical geometriesDental Materials, 2008
- Flexural strength of veneering ceramics for zirconiaJournal of Dentistry, 2008
- Prestresses in bilayered all‐ceramic restorationsJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2008
- State of the art of zirconia for dental applicationsDental Materials, 2008
- Analyses of layer-thickness effects in bilayered dental ceramics subjected to thermal stresses and ring-on-ring testsDental Materials, 2008
- An overview of zirconia ceramics: Basic properties and clinical applicationsJournal of Dentistry, 2007
- Influence of water, loading rate and bonder on the adhesion of porcelain to titaniumJournal of Dentistry, 2006
- All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical studyJournal of Oral Rehabilitation, 2005
- Analysis of Bi-Metal ThermostatsJournal of the Optical Society of America, 1925