Silica Fume Treatments as Means for Improving Durability of Glass Fiber Reinforced Cements
Author:
- 1 August 1989
- journal article
- Published by American Society of Civil Engineers (ASCE) in Journal of Materials in Civil Engineering
- Vol. 1 (3) , 167-183
Abstract
Treatments with silica fume slurry were applied to improve the durability of alkali resistant (AR) glass fiber reinforced cement composites (GFRC). Two treatments were studied: fiber treatment obtained by immersion of the reinforcing strand in the slurry, prior to their incorporation in the composite, and matrix modification of the matrix by replacing with 10% silica fume. Fiber treatment alone was found to be extremely effective, leading to 50% or more toughness retention after 5 to 9 months of accelerated aging. Additional modification of the matrix led to better performance, with the toughness retention exceeding 50%. Matrix modification alone did not yield any significant improvement. The effects of the silica fume treatments were discussed in terms of the microstructural and chemical aging mechanisms.Keywords
This publication has 5 references indexed in Scilit:
- Improvement of the durability of glass fiber reinforced cement using blended cement matrixCement and Concrete Research, 1984
- Developments in the assessment and performance of grc over 10 yearsComposites, 1982
- Properties of high-alumina cement reinforced with alkali resistant glass fibresJournal of Materials Science, 1981
- The use of accelerated ageing procedures to predict the long term strength of GRC compositesCement and Concrete Research, 1981
- Microstructure of glass fibre-reinforced cement compositesJournal of Materials Science, 1976