Oxidation behavior of bulk Ti3SiC2 at intermediate temperatures in dry air
- 1 February 2006
- journal article
- Published by Springer Nature in Journal of Materials Research
- Vol. 21 (2) , 402-408
Abstract
The isothermal oxidation behavior of bulk Ti3SiC2 at intermediate temperatures from 500 to 900 °C in flowing dry air was investigated. An anomalous oxidation with higher kinetics at lower temperatures was observed. This phenomenon resulted from the formation of microcracks in the oxide scales at low temperatures. The generation of these microcracks was caused by a phase change in the oxide products, i.e., the transformation of anatase TiO2 to rutile TiO2. This phase transformation resulted in tensile stress, which provided the driving force for the formation of the microcracks during oxidation. Despite the existence of microcracks, the intermediate-temperature oxidation of Ti3SiC2 generally obeyed the parabolic rate law and did not exhibit catastrophic destruction due to the fact that cracks occurring in the oxide layers were partially filled with amorphous SiO2. Therefore, further high oxidation kinetics was prevented.Keywords
This publication has 33 references indexed in Scilit:
- The structure and thermal stability of TiO2 grown by the plasma oxidation of sputtered metallic Ti thin filmsChemical Physics Letters, 2004
- Preparation of porous anatase titania filmMaterials Letters, 2004
- Understanding Polymorphic Phase Transformation Behavior during Growth of Nanocrystalline Aggregates: Insights from TiO2The Journal of Physical Chemistry B, 2000
- In-situ hot pressing/solid-liquid reaction synthesis of dense titanium silicon carbide bulk ceramicsMaterials Research Innovations, 1998
- Correlation Between Anatase-to-rutile Transformation and Grain Growth in Nanocrystalline Titania PowdersJournal of Materials Research, 1998
- Oxidation Of Ti3SiC2 in AirJournal of the Electrochemical Society, 1997
- Solid-state synthesis and characterization of the ternary phase Ti3SiC2Journal of Materials Science, 1994
- Oxidation behavior of monolithic TiN and TiN dispersed in ceramic matricesOxidation of Metals, 1993
- Oxidation Kinetics of Hafnium Carbide in the Temperature Range of 480° to 600°CJournal of the American Ceramic Society, 1992
- “PEST” degradation in beryllides, silicides, aluminides, and related compoundsJournal of Nuclear Materials, 1964