Abstract
An extrusion process was developed that is able to consistently produce large quantities of Mo-Si-B rods without the presence of defects. Binder removal from the extruded rods was studied in detail and it was determined that heating rates on the order of 0.02°/minute (1.2°/hour) are necessary to remove the binder without the formation of defects. This low heating rate resulted in debinding times in excess of 70 hours (approximately 3 days). Wicking was investigated as a means to decrease the time necessary for binder removal. Using 0.05μm alumina powder as a wicking agent, binder removal times were reduced to 10 hours with heating rates up to 1°/minute employed without defect formation. Once the extrusion process was complete the oxidation properties of the Tl-MoSi 2-MoB extruded phase assemblage was investigated. It was determined that this composition exhibits catastrophic oxidation or pesting in the temperature range of 660-760°C, resulting in the material turning to dust. Outside of this temperature range the composition is oxidatively stable. Continuous mass measurements were taken at 1,300, 1,450, and 1,600 C to determine the oxidation rate constants of this material. Parabolic rate constants of 6.9 x 10 -3, 1.3 x 10 -3, and 9.1 x 10 -3more » mg 2/cm 4/hr were determined for 1,300, 1,450, and 1,600 C respectively. « less
Funding Information
  • USDOE
  • DOE (W-7405-ENG-82)