Hold-time effects on elevated-temperature low-cycle-fatigue and crack-propagation behaviors of HAYNES® 188 superalloy
- 7 April 2009
- journal article
- research article
- Published by Springer Nature in Journal of Materials Science
- Vol. 44 (11) , 2945-2956
Abstract
No abstract availableKeywords
This publication has 24 references indexed in Scilit:
- Tensile-hold low-cycle-fatigue properties of solid-solution-strengthened superalloys at elevated temperaturesMaterials Science and Engineering: A, 2009
- Effects of temperature and hold time on creep-fatigue crack-growth behavior of HAYNES® 230® alloyMaterials Science and Engineering: A, 2006
- Hold time effects on low cycle fatigue behavior of HAYNES 230® superalloy at high temperaturesMaterials Science and Engineering: A, 2005
- Cyclic deformation behavior of HAYNES® HR-120® superalloy under low-cycle fatigue loadingMechanics of Materials, 2004
- Tensile hold low-cycle fatigue behavior of cobalt-based HAYNES® 188 superalloyScripta Materialia, 2001
- Creep-fatigue behaviour of CoCr22Ni22W14 in the temperature range 850 °C < T < 1200 °CMaterials Science and Engineering: A, 1997
- On the low cycle fatigue deformation of haynes 188 superalloy in the dynamic strain aging regimeScripta Metallurgica et Materialia, 1995
- A study of fatigue damage mechanisms in Waspaloy from 25 to 800°CMaterials Science and Engineering, 1984
- A Damage Function and Associated Failure Equations for Predicting Hold Time and Frequency Effects in Elevated Temperature, Low Cycle FatigueJournal of Testing and Evaluation, 1976
- The low cycle fatigue of three wrought nickel-base alloysMetallurgical Transactions, 1974