Noise Reduction of Amorphous SixGeyO1–x–yThin Films for Uncooled Microbolometers by Si3N4Passivation and Annealing in Vacuum

Authors:

Abstract
This paper presents the fabrication and reduction of noise voltage power spectral density (PSD) of Si x Ge y O 1-x-y uncooled infrared microbolometers with four different compositions. The noise reduction was achieved by passivating Si x Ge y O 1-x-y with Si 3 N 4 layers and by annealing the devices in vacuum at 200 °C, 250 °C, or 300 °C with different time intervals from 1 to 5 h. The voltage noise PSD was measured with a bias current between 0.07 and 0.6 μA before and after annealing. The lowest measured noise voltage PSD before annealing was on devices with Si 0.053 Ge 0.875 O 0.072 and Si 0.041 Ge 0.902 O 0.057 films. They were 7.42 × 10 -15 and 2.07 × 10 -14 V 2 /Hz at 23 Hz, respectively. The corresponding 1/f-noise coefficients, Kf , of the devices were 3.65 × 10 -14 and 3.01 × 10 -14 , respectively. The voltage noise PSD was reduced as the annealing time and temperature were increased. The lowest measured noise was 1.96 × 10 -14 V 2 /Hz at the corner frequency, 12 Hz, on a device with Si 0.034 Ge 0.899 O 0.067 film annealed at 300 °C for 4 h, before annealing the noise was 4.09 × 10 -13 V 2 /Hz at 12 Hz. This corresponds to a factor of 24 reduction of noise. The testing results demonstrate that annealing at higher temperature 300 °C reduced the low-frequency voltage noise PSD more than that of 200 °C and 250 °C temperatures.
Funding Information
  • U.S. Army Research Office (W911NF-09-1-0158)