ANALYSIS OF FRICTION STIR WELDING JOINTS ON HIGH DENSITY POLYETHYLENE (HDPE) DUE TO CHANGE IN MATERIAL TEMPERATURE AND SPINDLE ROTATION
- 11 December 2024
- journal article
- research article
- Published by MM Publishing, s.r.o. in MM Science Journal
- Vol. 2024 (6) , 7851-7857
Abstract
Friction stir welding (FSW) can be a solution in solving the problem of joining thermoplastic polymers which are difficult to do with fusion welding. Selection of the proper FSW connection parameters can produce optimal connection quality in HDPE material joints. In friction stir welding, the heat of welding is used to raise the temperature of the material from its initial state to the solid state temperature. If the material temperature (T0) is increased above room temperature (TRoom), while the FSW welding parameter is constant, then at a certain increase in T0 it will produce excess welding heat which results in excessive softening or even melting of the material being welded. Therefore, the material temperature setting (T0) becomes an important parameter FSW The process of connecting the HDPE plates with friction stir welding was carried out by varying the material temperature (T0 ) of TRoom, 50 0C, 75 0C and 100 0C. While the spindle rotation varies 2000 rpm and 2500 rpm. Other parameters controlled include the type of square butt joint, 5 mm HDPE plate thickness, 20 mm/min feed rate, 0.1 mm plunge depth, 20 mm tool shoulder diameter, 4.5 mm pin length and 6 mm pin diameter. The result is that the higher the spindle rotation and the material temperature during the welding process causes the FSW peak welding temperature to increase. The highest peak weld temperature was obtained at variations in material temperature (T0) 100 °C with a spindle rotation of 2500 rpm, which is 123.2 °C or 94% of the melting temperature of HDPE. The hardness of the weld nugged area is still lower than the hardness of the base material. The highest average tensile strength of the research variations was achieved at a spindle rotation speed of 2500 rpm and a material temperature of 75 °C of 16.8 MPa, higher than the average tensile strength of the base material which is 15.1 MPa.Keywords
This publication has 18 references indexed in Scilit:
- Friction Stir Welding for Joining of Polymers2018
- Influences of tool traverse speed on tensile properties of air cooled and water cooled friction stir welded AA2519-T87 aluminium alloy jointsJournal of Materials Processing Technology, 2016
- Influences of welding parameters on the quality and creep properties of friction stir welded polyethylene platesMaterials & Design (1980-2015), 2015
- Friction stir welding of thermoplastics using a newly designed toolMaterials & Design (1980-2015), 2014
- A Coupled Thermal/Material Flow Model of Friction Stir Welding Applied to Sc-Modified Aluminum AlloysMetallurgical and Materials Transactions A, 2012
- The optimization of friction stir welding process parameters to achieve maximum tensile strength in polyethylene sheetsMaterials & Design (1980-2015), 2012
- Evaluation of mechanical interlock effect on adhesion strength of polymer–metal interfaces using micro-patterned surface topographyInternational Journal of Adhesion and Adhesives, 2010
- Mechanical evaluation and thermal modelling of friction welding of mild steel and aluminiumJournal of Materials Processing Technology, 2010
- Effect of process parameters on thermal history and mechanical properties of friction stir weldsMaterials & Design (1980-2015), 2009
- In-process heat treatments to improve FS-welded butt jointsThe International Journal of Advanced Manufacturing Technology, 2008