Abstract
The ferromagnetic resistance anisotropy Δρ/ρ0=(ρ∥−ρ⊥)/ ρ0 of Co91Fe09 films with thickness t between 5 and 113 nm has been measured at 4.2 and 295 K. Here, ρ∥ and ρ⊥ are the resistivities when the magnetization is parallel and perpendicular to the current, and ρ0 is the zero‐field resistivity. Δρ/ρ0 is equal to 2.7% for t>40 nm at 4.2 K, but decreases fast for thinner films. This decrease is associated with an increase of surface scattering and grain‐boundary scattering. We plot Δρ/ρ0 vs ρB/ ρ0 where ρB is the resistivity of a bulk sample. This is the appropriate version for thin films of the ‘‘Parker plot,’’ based on Matthiessen’s rule. Our data form a straight line on this plot, in accordance with theory. Films of thickness ≂80 nm have been annealed at 300 °C, causing a reduction of lattice defects and an increase of Δρ/ρ0. The Parker plot shows that different scattering centers are important in annealed and unannealed samples. We also measured the compositional dependence of Δρ/ρ0 in thick CoxFe100−x films.

This publication has 11 references indexed in Scilit: