Through-thickness creep damage in a service-exposed header of 2.25Cr1 Mo steel
Authors:
- Rui WuRWRui Wu
- Rolf SandströmRSRolf Sandström
- Jan StoresundJSJan Storesund
- 1 August 1992
- journal article
- research article
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 10 (3) , 154-163
Abstract
A creep damage investigation was made on a service-exposed header of 2.25Cr 1Mo steel with a service time of 200 000 h. Weldments and the flanged parts at both outer and inner surfaces were studied as well as the damage in the through-thickness direction. Extensive cavitation was observed not only at the outer surface, but also well inside the component in the weldments. A model for the prediction of rupture position is introduced to explain the appearance of the observed creep damage.Keywords
This publication has 6 references indexed in Scilit:
- Creep behaviour of 2.25Cr1Mo steel from a service-exposed headerMaterials at High Temperatures, 1992
- Analysis of material exhaustion and damage by creepInternational Journal of Pressure Vessels and Piping, 1991
- Creep damage in welded joints of 0.5CrMoV steelHigh Temperature Technology, 1987
- Multiaxial Stress Rupture Testing and Compendium of Data for Creep Resisting SteelsJournal of Engineering Materials and Technology, 1982
- Remaining creep life estimation by strain assessment on plantInternational Journal of Pressure Vessels and Piping, 1982
- Creep rupture under multi-axial states of stressJournal of the Mechanics and Physics of Solids, 1972