Abstract
Reactively sputtered tungsten oxide (WO x ) was investigated as hole contact on n-type crystalline silicon. Varying the oxygen gas flow during sputtering enables variation of the WO x conductivity from 0.01 to 1000 Ω/cm, while the band bending at the interface and the implied fill factor (FF) change by 70 meV and 1.5%. Sputtered WO x shows higher resistivity and higher absorption in the visible range compared with indium-tin-oxide (ITO). Therefore, stacks of WO x and ITO are used in solar cells. It was found that at least 20 nm thick WO x is needed to prevent detrimental effects of the ITO work function on the band bending at the junction, the implied FF, and the real FF of solar cells. WO x hole contacts of different thicknesses and conductivity were applied in solar cells and it was found that the highest FF is achieved using about 20 nm thick interlayers of WO x with the highest possible conductivity. It was found that sputtering enables a drastic improvement of WO x /silicon solar cells compared with thermal evaporation, due to the precise control of the WO x conductivity. Unfortunately, the resistivity of the sputtered WO x is still limiting the FF of these devices.
Funding Information
  • European Commission through the Project NextBase (727523)
  • ERASMUS PLUS program of the French ERASMUS agency
  • Languedoc Roussillon Region

This publication has 28 references indexed in Scilit: