Limits to the preparation of superhard nanocomposites: Impurities, deposition and annealing temperature
Authors:
- S. VeprekSVS. Veprek
- M.G.J. Veprek-HeijmanMVM.G.J. Veprek-Heijman
- 1 November 2012
- journal article
- Published by Elsevier in Thin Solid Films
- Vol. 522, 274-282
Abstract
No abstract availableKeywords
This publication has 63 references indexed in Scilit:
- Critical review of claims for ultra-hardness in nanocomposite coatingsPhilosophical Magazine, 2012
- The location and effects of Si in (Ti1–xSix)Ny thin filmsJournal of Materials Research, 2009
- Industrial applications of superhard nanocomposite coatingsSurface and Coatings Technology, 2008
- The issue of the reproducibility of deposition of superhard nanocomposites with hardness of ≥50 GPaSurface and Coatings Technology, 2006
- Possible role of oxygen impurities in degradation of nc-TiN∕a-Si3N4 nanocompositesJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2005
- Different approaches to superhard coatings and nanocompositesThin Solid Films, 2005
- Degradation of superhard nanocomposites by built-in impuritiesJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2004
- Composition, nanostructure and origin of the ultrahardness in nc-TiN/a-Si3N4/a- and nc-TiSi2 nanocomposites with HV=80 to ≥105 GPaSurface and Coatings Technology, 2000
- A concept for the design of novel superhard coatingsThin Solid Films, 1995
- Ti-Si-N films prepared by plasma-enhanced chemical vapor depositionPlasma Chemistry and Plasma Processing, 1992