Abstract
A p-channel metal-ferroelectric-insulator-silicon field-effect transistor (FET) with a 300-nm-thick SrBi2Ta2O9 (SBT) ferroelectric film and a 10-nm-thick HfTaO layer on silicon substrate was fabricated and characterized. The device shows a nearly unchanged memory window of about 0.9 V after a 2 × 1011-cycles fatigue test, an on/off current ratio of more than 107, and a field-effect mobility of approximately 42 cm2/V · s. Moreover, a drain-current on/off ratio as high as 105 was obtained with a fixed gate voltage of 2.5 V after over a 105 -s elapsed time without any obvious degradation. These results may suggest that the Pt/SBT/HfTaO/Si FET is suitable for high-performance ferroelectric memory.

This publication has 21 references indexed in Scilit: