Thin film silicon n–i–p solar cells deposited by VHF PECVD at 100°C substrate temperature
Authors:
- M. BrinzaMBM. Brinza
- J.K. RathJRJ.K. Rath
- R.E.I. SchroppRSR.E.I. Schropp
- 1 June 2009
- journal article
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 93 (6-7) , 680-683