Abstract
The paper studies the dynamic recrystallization of nitrogen‐alloyed low‐nickel Fe–16Cr–xMn–4Ni–0.05C–0.17N stainless steel in dependence of Mn with different contents from 2 to 6 wt% by isothermal compression tests. The tests are performed at three temperatures 970, 1050, 1150 °C and three strain rates 0.1, 1, and 10 s−1 on a Gleeble HDS V40. By means of the experimental results, it could be shown that various Mn content has only a slight effect on the peak stress and peak strain. The critical stress indicating the onset of dynamic recrystallization is determined by second derivative of the third‐order polynomial. The dynamic recrystallization is modeled based on the JMAK equations, which is expanded by means of including the linear dependency of material constants of the Mn content. The predicted DRX curves exhibit good agreement with the experimental ones.