Effect of ultraviolet and temperature on mechanical properties of three dimension printed materials

Authors:
  • NANabaa Alaa Aldeen
    Nabaa Alaa Aldeen
  • BOBashar Owaid
    Bashar Owaid

Abstract
The aim of the research is to study the effect of temperature and ultraviolet radiation on polymers used in three-dimensional printing. Some important mechanical properties have been studied before and after exposure to accelerated weather conditions (temperature and ultraviolet radiation) by (accelerated weathering tester –model QVB\spray) device. We concentrated on three types of materials used in three-dimensional printing which are (polylactic acid, carbon filer, polylactic plus). The research problem was simulated by the high temperatures and UV radiation from the sun which is characterized the Iraqi climate throughout the year that affects the polymers in general by reducing the span and the deformity of the outer surface also lack of resistance to weather conditions. The three-dimensional printer (FDM) was used in practical term to print samples according to (ASTM D638) which leads to some mechanical properties results (yield point, max load, young modulus, max stress). The samples passed the examination stage successfully then the researchers printed the models according to the preliminary models data and the exposed to heat and ultraviolet radiation by the accelerated device of weather conditions for different periods ranging from (15, 35, 65) hours, after the exposure of the samples to the accelerated weather conditions and testing by tensile test obtained a series of results and the most important was the negative effects on the polymers used in the three-dimensional printing by these conditions also the deformation of the external surface of the samples and the lack of mechanical properties as shown in some of the following results: It was found that there was a negative effect on these materials where the highest strength was before exposure to the three substances that resisted the tension force imposed by the tensile device (1.616 for pla, 1.306 for cf, 1.802 for pla+) after exposure for 15 hours (1.364 for pla, 1.262 for cf, 1.522 for pla+. after exposure for 35 hours (1.154 for pla, 0.6293 for cf, 0.752 for pla+) after exposure for 65 hours it became (0.988 for pla, 0.6001 for cf, 0.562 for pla+).

This publication has 2 references indexed in Scilit: