Retrospective Study of Extensive Heat‐Pressed Ceramic Veneers after 36 Months
Authors:
- 26 September 2012
- journal article
- research article
- Published by Wiley in Journal of Esthetic and Restorative Dentistry
- Vol. 25 (1) , 42-52
Abstract
Statement of the Problem: The clinical performance of ceramic veneers is influenced by various clinical and material‐related factors.Purpose: Retrospective evaluation of extensive anterior ceramic veneers in the upper and lower jaw 36 months after placement in a private practice.Materials and Methods: Thirty‐seven patients (21 female, 16 male) were restored with adhesively luted extensive ceramic veneers made from a heat‐pressed ceramic (Cergo, DeguDent, Hanau, Germany). One dentist restored a total of 130 teeth (maxilla N = 76, mandible N = 54). Adhesive cementation was performed with an etch‐and‐rinse adhesive (Optibond FL, Kerr Hawe, Karlsruhe, Germany) and a dual‐curing composite cement.Results: After 36 months, the survival rate (in situ criteria) according to Kaplan–Meier was 95.1% (95% confidence interval [CI]: 0.88; 1). Reasons for failure were four ceramic fractures and one biological failure in five restored teeth. Of the restorations, 92.8% (95% CI: 0.86;1) were in service without any clinical intervention and rated successful after 36 months. Interventions were necessary in five cases (three recementations, two endodontic treatments). Clinical performance was not influenced by the veneer position (maxillar/mandibular, survival p = 0.3/success p = 0.4). Veneers with more than 50% of exposed dentin demonstrated a significantly increased risk (hazard ratio 10.6, p = 0.026) for a clinical intervention (recementation, endodontic treatment), whereas no effect on the survival rate could be detected (p = 0.17).Conclusions: After 36 months of clinical service, extensive veneer restorations made of a pressable ceramic showed a comparable survival and success rate in the upper and lower jaw. Large areas of exposed dentin (>50%) were associated with lower success rates.Clinical Significance: Mandibular ceramic veneers made using a heat‐pressed ceramic offer the same clinical reliability as do veneers on anterior maxillary teeth. Dentin exposure significantly affects the clinical performance of heat‐pressed ceramic veneers.Keywords
This publication has 19 references indexed in Scilit:
- Ten-year outcome of porcelain laminate veneers placed within the general dental services in England and WalesJournal of Dentistry, 2009
- CLINICAL CONSIDERATIONS FOR RESTORING MANDIBULAR INCISORS WITH PORCELAIN LAMINATE VENEERSJournal of Esthetic and Restorative Dentistry, 2008
- Midterm results of a 5-year prospective clinical investigation of extended ceramic veneersDental Materials, 2008
- A systematic review of the survival and complication rates of all‐ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part I: single crownsClinical Oral Implants Research, 2007
- To what extent does the longevity of fixed dental prostheses depend on the function of the cement? Working Group 4 materials: cementationClinical Oral Implants Research, 2007
- PORCELAIN VENEER OUTCOMES, PART IJournal of Esthetic and Restorative Dentistry, 2006
- Reprint of Criteria for the clinical evaluation of dental restorative materialsClinical Oral Investigations, 2005
- Clinical performance of porcelain laminate veneers. A retrospective evaluation over a period of 6.5 yearsJournal of Oral Rehabilitation, 1997
- Ceramic Laminate Veneers: Continuous Evolution of IndicationsJournal of Esthetic and Restorative Dentistry, 1997
- A longitudinal study of the clinical performance of porcelain veneersBritish Dental Journal, 1993