A rheological study on non-rubber component networks in natural rubber
- 24 September 2015
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (111) , 91742-91750
Abstract
Phospholipids and proteins were separately removed as the main non-rubber components to individually study their effect on the structure and properties of the rubber. Fourier Transform Infrared Spectroscopy (FTIR) and 1H nuclear magnetic resonance spectroscopy (1H-NMR) were used to characterize the chemical structure and the residual non-rubber component. A rheology study and stress relaxation measurements were used to study the role that non-rubber components play in natural networks. A rheological study showed that natural rubber (NR) and deproteinized natural rubber (DPNR) exhibited similar dynamic modulus at 170 °C. The lack of superposition in van Gurp–Palmen (vGP) curves at different temperatures for NR and DPNR, together with the shape of vGP curves, proved that long chain branching was mainly constructed by phospholipids. Stress relaxation measurements at room temperature were fitted with the Maxwell model and showed that the NR relaxation curve underwent a quick decrease and then came to an equilibrium stress retention of 58%, which is about 3 times higher than that of DPNR, indicating that proteins in NR contributed to the network structure at room temperature. Combining molecular dynamic studies, the interaction of proteins and phospholipids in non-rubber networks was proposed.Keywords
This publication has 48 references indexed in Scilit:
- Rubber Elongation Factor (REF), a Major Allergen Component in Hevea brasiliensis Latex Has Amyloid PropertiesPLOS ONE, 2012
- Structure and properties of polylactide/natural rubber blendsMaterials Chemistry and Physics, 2011
- Living Radical Polymerization of Isoprene via the RAFT ProcessMacromolecules, 2007
- Stress Relaxation of End-Linked Polydimethylsiloxane Elastomers with Long Pendent ChainsMacromolecules, 2005
- A new semi-phenomenological approach to predict the stress relaxation behavior of thermoplastic elastomersPolymer, 2005
- An Efficient Gadolinium Metallocene-Based Catalyst for the Synthesis of Isoprene Rubber with Perfect 1,4-Cis Microstructure and Marked Reactivity Difference between Lanthanide Metallocenes toward Dienes As Probed by Butadiene−Isoprene Copolymerization CatalysisMacromolecules, 2004
- Molecular structure of high melt strength polypropylene and its application to polymer designPolymer, 2003
- Synthesis of Combs, Centipedes, and Barbwires: Poly(isoprene-graft-styrene) Regular Multigraft Copolymers with Trifunctional, Tetrafunctional, and Hexafunctional Branch PointsMacromolecules, 2002
- Stress relaxation of peroxide and sulfur vulcanizates of natural rubberJournal of Polymer Science, 1955
- Stress Relaxation of Natural and Synthetic Rubber StocksJournal of Applied Physics, 1944