Statistical analysis and theoretical predictions of the tensile-strength retention of glass fiber-reinforced polymer bars based on resin type
- 9 February 2018
- journal article
- research article
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 52 (21) , 2929-2948
Abstract
This paper presents experimental investigation, statistical analysis, and theoretical predictions of tensile-strength retention of glass fiber-reinforced polymer bars, made with vinyl-ester, polyester, or epoxy resins. The durability of glass fiber-reinforced polymer bars was evaluated as a function of time of immersion in alkaline solution. The aging of the three glass fiber-reinforced polymer bar types consisted of immersion glass fiber-reinforced polymer bar samples in an alkaline solution (up to 5000 h) at different elevated exposure temperatures. Subsequently, the physical and tensile properties of the unconditioned bars were compared with that of the conditioned bars to assess the durability performance of the glass fiber-reinforced polymer bars. Microstructure of all of the glass fiber-reinforced polymer bar types was investigated with scanning electron microscopy, energy dispersive spectroscopy, and Fourier transform infrared spectroscopy for both the conditioned and unconditioned cases, to qualitatively explain the experimental results and to assess changes and/or degradation in the glass fiber-reinforced polymer bars. In addition, the long-term performance of glass fiber-reinforced polymer bars was assessed considering the effect of service years, environmental humidity, and seasonal temperature fluctuations. The test results showed that the tensile strength of the glass fiber-reinforced polymer bars was affected by increased immersion time at higher temperatures and the reduction in tensile strength was statistically significantly dependent on the type of resin system. The prediction approach of the glass fiber-reinforced polymer bars based on the environmental reduction factor ( CE) after 200 years indicated that the CE values for vinyl-ester, epoxy, and polyester glass fiber-reinforced polymer bars can be conservatively recommended to 0.81, 0.75, and 0.71, respectively, for a moisture-saturated environment (relative humidity = 100%) and at 30℃. The polyester glass fiber-reinforced polymer bars experienced greater debonding at the fiber–resin interface than the vinyl-ester and epoxy glass fiber-reinforced polymer bars.Keywords
This publication has 30 references indexed in Scilit:
- Combined effects of saline solution and moist concrete on long-term durability of GFRP reinforcing barsConstruction and Building Materials, 2013
- Ageing of carbon/epoxy and carbon/vinylester composites used in the reinforcement and/or the repair of civil engineering structuresComposites Part B: Engineering, 2012
- Tensile properties degradation of glass fiber-reinforced polymer bars embedded in concrete under severe laboratory and field environmental conditionsJournal of Composite Materials, 2012
- Short-term durability test for GFRP rods under various environmental conditionsComposite Structures, 2008
- Chemical Durability and Mechanical Properties of Alkali-proof Basalt Fiber and its Reinforced Epoxy CompositesJournal of Reinforced Plastics and Composites, 2008
- Effect of Environmental Exposure on the Mechanical and Bonding Properties of Hybrid FRP Reinforcing Bars for Concrete StructuresJournal of Composite Materials, 2006
- Durability of FRP rods for concrete structuresConstruction and Building Materials, 2004
- A model specification for FRP composites for civil engineering structuresConstruction and Building Materials, 2003
- Interactions of water with unsaturated polyester, vinyl ester and acrylic resinsPolymer, 1992
- Water damage in glass fibre/resin compositesProceedings of the Royal Society of London. A. Mathematical and Physical Sciences, 1969