Plasma impact on 193 nm photoresist linewidth roughness: Role of plasma vacuum ultraviolet light
Authors:
- 9 March 2009
- journal article
- conference paper
- Published by AIP Publishing in Applied Physics Letters
- Vol. 94 (10) , 103111
Abstract
193 nm photoresist patterns printed by optical lithography are known to present significant linewidth roughness (LWR) after the lithographic step that is partially transferred into the underlayers during plasma etching processes. In this study, we identify the factors that impact the photoresist pattern sidewalls roughness during plasma exposure. Among them, plasma vacuum ultraviolet light (110–210 nm) is shown to be the main contributor to the LWR decrease induced by plasma etching processes. In this paper, we also demonstrate the strong correlation between LWR obtained after plasma exposure and the surface roughening mechanisms taking place on top of the resist patterns.Keywords
This publication has 12 references indexed in Scilit:
- Study of 193nm photoresist degradation during short time fluorocarbon plasma exposures. II. Plasma parameter trends for photoresist degradationJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2008
- Linewidth roughness transfer measured by critical dimension atomic force microscopy during plasma patterning of polysilicon gate transistorsJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2008
- Synergistic effects of vacuum ultraviolet radiation, ion bombardment, and heating in 193nm photoresist roughening and degradationApplied Physics Letters, 2008
- Advances in CD-AFM scan algorithm technology enable improved CD metrology2007
- Changes of chemical nature of photoresists induced by various plasma treatments and their impact on LWR2006
- From CD to 3D sidewall roughness analysis with 3D CD-AFM2005
- Line edge roughness reduction by plasma curing photoresists2005
- Deposition control for reduction of 193nm photoresist degradation in dielectric etchingJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2005
- Effect of thin-film imaging on line edge roughness transfer to underlayers during etch processesJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2004
- Sub-0.1 μm nitride hard mask open process without precuring the ArF photoresistJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 2003