Hard and Tough Boron Suboxide Based Composites
Authors:
- 10 October 2006
- conference paper
- Published by Trans Tech Publications, Ltd. in Advances in Science and Technology
- Vol. 45, 1745-1750
Abstract
Boron Suboxide (B6O) powder was synthesized at temperatures of about 1400 oC from the reaction of boron and boric acid powders. The synthesized B6O powders were hot pressed at 1900 oC and at pressures of 50 MPa. Additionally to pure B6O materials, composites with Aluminum were prepared. The microstructure and properties of the sintered compacts were investigated. The addition of Aluminum in the composites results in the formation of an additional Aluminum Borate phase. The composites showed a similar hardness (~30GPa) as the pure B6O samples but an increased fracture toughness (~3.5MPa.m1/2).Keywords
This publication has 8 references indexed in Scilit:
- Boron suboxide: As hard as cubic boron nitrideApplied Physics Letters, 2002
- High pressure consolidation of B6O-diamond mixturesJournal of Materials Science, 2001
- B6O–c‐BN Composites Prepared by High‐Pressure SinteringJournal of the American Ceramic Society, 2000
- Microstructure and mechanical properties of B6O-B4C sintered composites prepared under high pressureJournal of Materials Science, 2000
- High Pressure Sintering of B6O Powder and Properties of Sintered CompactJournal of the Society of Materials Science, Japan, 1998
- High-Pressure, High-Temperature Synthesis and Characterization of Boron Suboxide (B6O)Chemistry of Materials, 1998
- Superhard boron-rich borides and studies of the BCN systemMaterials Science and Engineering: A, 1996
- A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack MeasurementsJournal of the American Ceramic Society, 1981