Mechanical‐Alloying‐Assisted Synthesis of Ti 3 SiC 2 Powder
Authors:
- 1 April 2002
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 85 (4) , 1004-1006
Abstract
Mechanical alloying (MA) has been used to synthesize Ti 3 SiC 2 powder from the elemental Ti, Si, and C powders. The MA formation conditions of Ti 3 SiC 2 were strongly affected by the ball size for the conditions used. MA using large balls (20.6 mm in diameter) enhanced the formation of Ti 3 SiC 2 , probably via an MA‐triggered combustion reaction, but the Ti 3 SiC 2 phase was not synthesized only by the MA process using small balls (12.7 mm in diameter). Fine powders containing 95.8 vol% Ti 3 SiC 2 can be obtained by annealing the mechanically alloyed powder at relatively low temperatures.Keywords
This publication has 19 references indexed in Scilit:
- Mechanical properties of polycrystalline Ti3SiC2 at ambient and elevated temperaturesActa Materialia, 2001
- Processing and Mechanical Properties of Ti 3 SiC 2 : II, Effect of Grain Size and Deformation TemperatureJournal of the American Ceramic Society, 1999
- Mechanochemical Synthesis of Lead Zirconate Titanate from Mixed OxidesJournal of the American Ceramic Society, 1999
- Field-activated pressure-assisted combustion synthesis of polycrystalline Ti3SiC2Journal of Materials Research, 1999
- Synthesis of Highly Dense Ti3SiC2 by HIP and Its CharacterizationJournal of the Society of Materials Science, Japan, 1998
- Synthesis and Characterization of a Remarkable Ceramic: Ti3SiC2Journal of the American Ceramic Society, 1996
- Synthesis and high temperature mechanical properties of Ti3SiC2/SiC compositeJournal of Materials Science, 1995
- Synthesis of Titanium Silicon CarbideJournal of the American Ceramic Society, 1995
- Ti3SiC-based materials prepared by HIP-SHS techniquesMaterials Letters, 1995
- Chemically vapor deposited Ti3SiC2Materials Research Bulletin, 1987